Hafif Agregalı Betonların Mekanik Özelikleri Ve Isı Yalıtımı

dc.contributor.advisor Taşdemir, Canan tr_TR
dc.contributor.author Konuk, Hakan tr_TR
dc.contributor.department Yapı Mühendisliği tr_TR
dc.contributor.department Structural Engineering en_US
dc.date 2003 tr_TR
dc.date.accessioned 2015-12-01T13:54:44Z
dc.date.available 2015-12-01T13:54:44Z
dc.description Tez (Yüksek Lisans) -- İstanbul Teknik Üniversitesi, Fen Bilimleri Enstitüsü, 2003 tr_TR
dc.description Thesis (M.Sc.) -- İstanbul Technical University, Institute of Science and Technology, 2003 en_US
dc.description.abstract Tane boyutu 2-16 mm. olan ponza hafif agregası Nevşehirden getirildi. Homojen hafif agrega elde etmek için sadece suda yüzen taneler beton dökümünde kullanıldı. Ponza agreganın su emmesi, 30 dakikadan sonra kuru ağırlığının %15’iydi. Karışım oranlarının hesaplanmasında mutlak hacim yöntemi kullanıldı. Ponza agregalı betonların taze birim ağırlığı 700 ile 1900 kg/m3 arasında 200 kg/m3 adımlarla değişmekteydi. Böylece 7 beton karışımı hazırlandı. Karışımların hepsinde etkin su/çimento oranı 0.43’dü. Maksimum agrega boyutu 16mm.’de sabit tutuldu. Agrega karışımının granülometri eğrisi A16-B16 referans eğrilerinin arasındaydı. Yaklaşık aynı işlenebilmeyi sağlamak için de süperakışkanlaştırıcı katkı kullanıldı. Düşük birim ağırlığa sahip (700 kg/m3, 900 kg/m3, 1100 kg/m3 ve 1300 kg/m3) betonlarda hava sürükleyici katkı kullanıldı. 700 kg/m3 birim ağırlığa sahip betonlarda, birim ağırlığı düşürmek için kum kullanılmadı. Bu çalışmada üretilen ponza hafif agregalı betonlarda, betonların birim ağırlığı ile basınç dayanımları arasında iyi bir lineer ilişki bulunmaktadır. “Elastisite modülü” ile (birim ağırlık)3/2 x (basınç dayanımı)1/2 arasında 0.99 korelasyon katsayısına sahip iyi bir ilişki elde edildi. Normal agrega yerine ponza hafif agrega kullanılmasıyla basınç dayanımları 1.4 - 18.7 MPa. ve elastisite modülleri de 1.6 - 19.5 GPa arasında oldu. 900 kg/m3, 1100 kg/m3 ve 1300 kg/m3 birim ağırlığa sahip betonların ısı iletim katsayısı (), plaka metodu test tekniği ile belirlendi. Deney sonuçları ile gaz betonlar için geliştirilen = -0.011 + 0.00027 x , (=birim ağırlık, kg/m3) bağıntısı kullanılarak hesaplanan sonuçlar arasında iyi bir lineer ilişki vardır. tr_TR
dc.description.abstract Pumice lightweight aggregate brought from Nevşehir and had a size range of 2 to 16 mm. In order to obtain a homogeneous lightweight aggregate, only particles that floated on water were used in the casting of the concrete. The water absorption of the Pumice aggregate after 30 minutes was 15 percent with respect to its dry weight. The absolute volumes was used in calculating the mix proportions. The fresh unit weights of pumice aggregate concretes were changed from 700 to 1900 kg/m3 in steps of 200 kg /m3. Thus seven concrete mixtures were obtained. All seven mixtures had an effective water-cement ratio of 0.43. The maximum particle size of aggregate was kept constant at 16 mm. The grading curve of combined aggregate was chosen between A16-B16. A superplasticiser was used to maintain approximately the same workability. An air-entraining agent was used in concretes with the unit weight (700,900,110,1300 kg/m3) in order to reduce the unit weight of the concrete. No sand was used in the concrete with a unit weight of 700 kg/m3. For the pumice lightweight aggregate concretes produced in this investigation, there is a good linear relation between compressive strength and unit weight of concrete. Good correlation between the “modulus of elasticity” and “(unitweight) 3/2 x (compressive strength) ½” is also obtained with a correlation coefficient of 0.99. The replacement of normal aggregate by the pumice lightweight aggregate results in compressive strengths ranging from 1.4 to 18.7 MPa and modulus of elasticity from 1.6 to 19.5 Gpa. The thermal conductivity coefficient of pumice concretes with the unit weights of 900,1100 and 1300 kg/m3 were determined using a plate test technique. There is a good linear relation between the experimental values obtained and the calculated values using the relation of  = 0,00027 x  - 0,011 developed for autoclaved aerated concretes, where  is the unit weight in kg/m3. en_US
dc.description.degree Yüksek Lisans tr_TR
dc.description.degree M.Sc. en_US
dc.identifier.uri http://hdl.handle.net/11527/10808
dc.publisher Fen Bilimleri Enstitüsü tr_TR
dc.publisher Institute of Science and Technology en_US
dc.rights İTÜ tezleri telif hakkı ile korunmaktadır. Bunlar, bu kaynak üzerinden herhangi bir amaçla görüntülenebilir, ancak yazılı izin alınmadan herhangi bir biçimde yeniden oluşturulması veya dağıtılması yasaklanmıştır. tr_TR
dc.rights İTÜ theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. en_US
dc.subject : Hafif Beton tr_TR
dc.subject Hafif Agrega tr_TR
dc.subject Pomza Agregası tr_TR
dc.subject Isı İletkenlik tr_TR
dc.subject Lightweight Concrete en_US
dc.subject Lightweight Aggregate en_US
dc.subject Pumice Aggregate en_US
dc.subject Thermal Insulation en_US
dc.title Hafif Agregalı Betonların Mekanik Özelikleri Ve Isı Yalıtımı tr_TR
dc.title.alternative Thermal Insulation And Mechanical Properties Of Lightweigt Agregate Concretes en_US
dc.type Master Thesis en_US
Dosyalar
Orijinal seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.alt
Ad:
1508.pdf
Boyut:
2.19 MB
Format:
Adobe Portable Document Format
Açıklama
Lisanslı seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.placeholder
Ad:
license.txt
Boyut:
3.14 KB
Format:
Plain Text
Açıklama