Eskişehir-kaymaz Epitermal Altın Cevherleri Üzerinde Çevreye Duyarlı Nitelikli Ön Zenginleştirme Yöntemlerinin Araştırılması

dc.contributor.advisor Güney, Ali tr_TR
dc.contributor.author Bayoğlu, Yağmur tr_TR
dc.contributor.authorID 10028351 tr_TR
dc.contributor.department Cevher ve Kömür Hazırlama tr_TR
dc.contributor.department Mineral and Coal Processing en_US
dc.date 2014 tr_TR
dc.date.accessioned 2014-02-19 tr_TR
dc.date.accessioned 2015-08-12T14:01:01Z
dc.date.available 2015-08-12T14:01:01Z
dc.date.issued 2014-02-20 tr_TR
dc.description Tez (Yüksek Lisans) -- İstanbul Teknik Üniversitesi, Fen Bilimleri Enstitüsü, 2014 tr_TR
dc.description Thesis (M.Sc.) -- İstanbul Technical University, Institute of Science and Technology, 2014 en_US
dc.description.abstract Bu çalışma kapsamında 4,51 ppm Au ve 13 ppm Ag içeren ve yapılan mineralojik incelemeler sonucunda % 95 ini kuvars, % 4 ünü demir içeren mineraller ve % 1 lik kısmını ise barit, pirit ve Ni-Zn-Cu sülfürlerden oluştuğu anlaşılanEskişehir Kaymaz bölgesine ait altın cevherlerinin zenginleştirmesine yönelik olarak, ilk aşamada bilyalı değirmende kullanılarak yapılan öğütme işlemi sonrası klasik flotasyon yöntemi ile uygun tane boyutu, flotasyon süresi,reaktif türü belirlenmiş, ikinci aşamada ise elde edilen en uygun flotasyon koşullarında yüksek altın içerikli konsantre eldesine yönelik deneyler gerçekleştirilmiştir. 250 g/t Aerophine 3418A ve 250 g/t Aero 208 kollektörleri kullanılarak yapılan kademeli flotasyon deneyleri sonucunda; 187 ppm Au içerikli konsantre % 54,2 verimle elde edilmiştir. KAX+ATP kolektörleri ile yapılan deneylerde ise 99,4 ppm Au içerikli konsantre % 57,3 verimle elde edilmiş, artık içeriği 1,98 ppm düzeyinde kaldığı tespit edilmiştir. tr_TR
dc.description.abstract In the firstphaseofthisstudy,appropriate grain size, floatation time and reaction type was determined by grinding in ball mills followed by classic floatation of Eskişehir-Kaymaz region gold ores wihch were determined to contain 4.51 ppm Au and 13 ppm Ag and was determined to consist of 95% quartz,%4 iron containing minerals and %1 barite, pyrite and Ni-Zn-Cu sulphurs by mineralogic investigation. Experiments to obtain high gold content concentrate in the most appropriate floatation contidions were made in the second phase. 187 ppm Au was obtained by 54.2% efficiency by using 250 g/t Aerophine 3418A and 250 g/t Aero 208 as collector. 99.4 ppm Au was obtained by 57.3% efficiency by using KAX+ATP as collector and waste content was determined to be 1.98 ppm en_US
dc.description.degree Yüksek Lisans tr_TR
dc.description.degree M.Sc. en_US
dc.identifier.uri http://hdl.handle.net/11527/8390
dc.publisher Fen Bilimleri Enstitüsü tr_TR
dc.publisher Institute of Science and Technology en_US
dc.rights İTÜ tezleri telif hakkı ile korunmaktadır. Bunlar, bu kaynak üzerinden herhangi bir amaçla görüntülenebilir, ancak yazılı izin alınmadan herhangi bir biçimde yeniden oluşturulması veya dağıtılması yasaklanmıştır. tr_TR
dc.rights İTÜ theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. en_US
dc.subject ALTIN tr_TR
dc.subject FLOTASYON tr_TR
dc.subject ÖN ZENGİNLEŞTİRME tr_TR
dc.subject GOLD en_US
dc.subject FLOATATION TIME en_US
dc.subject GRINDING en_US
dc.title Eskişehir-kaymaz Epitermal Altın Cevherleri Üzerinde Çevreye Duyarlı Nitelikli Ön Zenginleştirme Yöntemlerinin Araştırılması tr_TR
dc.title.alternative An Investigation Of Environmentally Friendly Pre-enrichment Methods On Eskişehir And Kaymaz Epithermal Gold Ores en_US
dc.type Master Thesis en_US
Dosyalar
Orijinal seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.alt
Ad:
14334.pdf
Boyut:
1.96 MB
Format:
Adobe Portable Document Format
Açıklama
Lisanslı seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.placeholder
Ad:
license.txt
Boyut:
3.16 KB
Format:
Plain Text
Açıklama