Alüminyum Altlık Üzerine Isıl Püskürtme Yöntemiyle Kaplanan Seramik Ve Seramik-polimer Kaplamaların Aşınma Davranışlarının İncelenmesi

dc.contributor.advisor Kayalı, E. Sabri tr_TR
dc.contributor.author Akın, Ufuk tr_TR
dc.contributor.department Malzeme tr_TR
dc.contributor.department Materials en_US
dc.date 2003 tr_TR
dc.date.accessioned 2015-09-11T11:16:33Z
dc.date.available 2015-09-11T11:16:33Z
dc.description Tez (Yüksek Lisans) -- İstanbul Teknik Üniversitesi, Fen Bilimleri Enstitüsü, 2003 tr_TR
dc.description Thesis (M.Sc.) -- İstanbul Technical University, Institute of Science and Technology, 2003 en_US
dc.description.abstract Bu çalışmada ticari saflıktaki alüminyum üzerine alevle püskürtme yöntemiyle kaplanan dört farklı oksit seramik kaplamanın (Cr2O3, ZrO2CaO, Al2O3, Al2O3TiO2) ve bu kaplamaların üzerine daldırma yöntemiyle teflon kaplanarak oluşturulan seramik/teflon karma kaplamaların kuru kayma koşulundaki aşınma davranışları, farklı yükler etkisinde, karşı malzeme olarak alümina ve çelik bilyeler kullanılarak salınım hareketli aşınma test cihazında ayrı ayrı incelenmiştir. İncelenen seramik kaplamalar arasından Cr2O3 kaplama en sert kaplama olup, her iki bilyeye karşı yapılan aşınma deneylerinde en yüksek aşınma direncini göstermiştir. Alümina bilye ile yapılan deneylerde aşınma direncinin büyükten küçüğe sıralaması Cr2O3, ZrO2CaO, Al2O3 ve Al2O3TiO2 iken çelik bilyede bu sıralama Cr2O3, Al2O3TiO2, Al2O3 ve ZrO2CaO şeklindedir. Seramik kaplamaların üzerinde teflon tabaka oluşturulması sürtünme katsayısını büyük ölçüde düşürerek 0.1 değerinin altına indirmiştir. Bu sayede aşınma azalmış ve kaplamaların servis ömrü artmıştır. İncelenen seramik kaplamalar arasında en az aşınan Cr2O3 ’ün üzerine teflon kaplanmasıyla elde edilen Cr2O3/teflon karma kaplama, diğer karma kaplamalarla karşılaştırıldığında en yüksek aşınma direncini göstermiştir. tr_TR
dc.description.abstract In this study, wear behaviours of four different oxide-ceramic coatings (Cr2O3, ZrO2CaO, Al2O3 and Al2O3TiO2) performed by flame spraying on commercial purity aluminum and teflon coatings produced by dipping on these oxide-ceramic coatings to make combined coating were investigated separately under dry sliding conditions with different loads and counterfaces (alumina and steel ball) by using reciprocating wear tester. Cr2O3 coating, the hardest coating among the ceramic coatings, showed the best wear resistance in both alumina and steel balls. In wear tests performed alumina ball, the highest wear resistance is followed by Cr2O3, ZrO2CaO, Al2O3 and Al2O3TiO2, respectively. In the stell ball, however, the highest wear resistance is followed by Cr2O3, Al2O3TiO2, Al2O3 and ZrO2CaO, respectively. In the case of aplication of teflon on the ceramic coatings, friction coefficient became less quantities (&#61549;<0.1). Thus, less wear and more service lifetime was provided. Cr2O3/teflon combined coating obtained by applying teflon layer on Cr2O3 coating, which is the least worn among the investigated ceramic coatings, exhibited highest wear resistance when compared with the other combined coatings. en_US
dc.description.degree Yüksek Lisans tr_TR
dc.description.degree M.Sc. en_US
dc.identifier.uri http://hdl.handle.net/11527/9293
dc.publisher Fen Bilimleri Enstitüsü tr_TR
dc.publisher Institute of Science and Technology en_US
dc.rights İTÜ tezleri telif hakkı ile korunmaktadır. Bunlar, bu kaynak üzerinden herhangi bir amaçla görüntülenebilir, ancak yazılı izin alınmadan herhangi bir biçimde yeniden oluşturulması veya dağıtılması yasaklanmıştır. tr_TR
dc.rights İTÜ theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. en_US
dc.subject Aşınma tr_TR
dc.subject Karma Kaplama tr_TR
dc.subject Seramik Kaplama. tr_TR
dc.subject Ceramic Coating en_US
dc.subject Combined Coating en_US
dc.subject Wear. en_US
dc.title Alüminyum Altlık Üzerine Isıl Püskürtme Yöntemiyle Kaplanan Seramik Ve Seramik-polimer Kaplamaların Aşınma Davranışlarının İncelenmesi tr_TR
dc.title.alternative Investigation Of Wear Behavior Of Thermally Sprayed Ceramic And Ceramic-polymer Coatings On Aluminum en_US
dc.type Master Thesis en_US
Dosyalar
Orijinal seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.alt
Ad:
1434.pdf
Boyut:
3 MB
Format:
Adobe Portable Document Format
Açıklama
Lisanslı seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.placeholder
Ad:
license.txt
Boyut:
3.14 KB
Format:
Plain Text
Açıklama