Beypazarı Ve Kazan Trona Cevherlerinin Flotasyon Ve Manyetik Ayırma Yöntemleriyle Zenginleştirilmesi

dc.contributor.advisor Çelik, Mehmet Sabri tr_TR
dc.contributor.author Matazimov, Daniyar tr_TR
dc.contributor.department Cevher Kömür Hazırlama ve Değerlendirme tr_TR
dc.contributor.department Coal and Mineral Processing en_US
dc.date 2005 tr_TR
dc.date.accessioned 2008-02-29 tr_TR
dc.date.accessioned 2015-11-19T12:27:34Z
dc.date.available 2015-11-19T12:27:34Z
dc.description Tez (Yüksek Lisans) -- İstanbul Teknik Üniversitesi, Fen Bilimleri Enstitüsü, 2005 tr_TR
dc.description Thesis (M.Sc.) -- İstanbul Technical University, Institute of Science and Technology, 2005 en_US
dc.description.abstract u çalışmada, Beypazarı ve Kazan trona cevherlerinin flotasyon yöntemiyle trona içeriğinin yükseltilmesi çalışmaları yapılarak, yüksek trona içeriğine sahip Beypazarı trona cevherinin % 65 PKO, 2.50 kg/ton DAH miktarı, 6.25 kg/ton gazyağı miktarı ve 90 saniye flotasyon süresinde optimum verim elde edilmiştir. Düşük trona içeren Kazan trona cevherinin iki farklı boyut grubu (-0,5+0,212 mm ve -0,212+0,038 mm) için DAH miktarına bağlı olarak yapılan flotasyon çalışmalarda, optimim DAH mikarının -0,5+0,212 mm boyut grubu için 2,5 kg/ton, -0,212+0,038 mm boyut grubu için de 5 kg/ton olduğu elde edilmiştir. Beypazarı ve Kazan trona cevherlerinin manyetik ayırma ile ön zenginleştirmeye de tabi tutulmuştur. Manyetik ayırma sonucu -1+0,5 mm ve -0,5+0,212 mm tane boyutlarında Beypazarı trona cevherlerinin trona içeriği % 97,20’ye yükseltilmiştir. Kazan trona cevherinin manyetik ayırma sonucu -0,5+0,212 mm tane boyutu için kısmen zenginleşme olmuştur, -0,212+0,038 mm tane boyutu için ise zenginleşme görülmemiştir. Özetle, elde edilen flotasyon sonuçları özellikle düşük trona içeren Kazan tronası için ümit vaat etmektedir. İyi bir optimizasyon ile manyetik ayırma işlemi de flotasyon öncesi bir ön zenginleştirme işlemi olarak dikkate alınması da öngörülmüştür. tr_TR
dc.description.abstract This study aims to remove as much impurity as possible from ‘Beypazarı’ and ‘Kazan’ trona ores by flotation and magnetic separation methods. The impurities in the Beypazarı trona ore sample of –1+0,5 mm in size did not float when the conditioning of trona with the emulsion composed of DAH as collector and kerosene as emulsifier was prepared in a separate conditioning tank. It was found that the addition of some brine during the condition made the impurities float. Because of this observation brine was added to the conditioning tank throughout the experiments. Experiments made as a functions of pulp density, amount of DAH collector and kerosene, and flotation time. In summary, the flotation process of trona under the conditions of 65 % by weight, 2.5 kg/t DAH collector, 6.25 kg/ton kerosene and 90 second flotation time gave the best results and the content of trona increased from % 95,92 to % 99,27 with a recovery of 73,08 %. Because the trona content of Kazan ore (55 %) is less than Beypazarı trona ore the amount of collector has been studied. The two size groups (-0,5+0,212 mm and 0,212+0,038 mm) of ore were subjected to flotation with the aim of optimizing the amount of DAH and kerosene; 2,5 kg/ton and 5 kg/ton, respectively were found to be the optimum. While the -0,5+0,212 mm trona ore was upgraded to % 91,75 % with a yield of 82,27 %, –0,212+0,038 mm trona was enriched to 92,13 % with a yield of 61,88 %. Magnetic separation method was applied to both Beypazarı and Kazan trona ores. Beypazarı trona prepared in –0,5+0,212 mm and –0,212+0,038 mm size fractions. The non-magnetic product was upgraded to 97,20 % with a yield of 71,08 % and 64,43 %, respectively. Magnetic separation of Kazan trona ore exhibited different results. –0,5+0,212 mm trona ore sample was not much successful despite excellent visual colour separation. -05+0.038 mm size fraction produced better results but not sufficient. It was found that although colour separation was unusually successful, trona is only partly liberated. Therefore, middlings require further size reduction to enable better grade and recoveries. en_US
dc.description.degree Yüksek Lisans tr_TR
dc.description.degree M.Sc. en_US
dc.identifier.uri http://hdl.handle.net/11527/10522
dc.publisher Fen Bilimleri Enstitüsü tr_TR
dc.publisher Institute of Science and Technology en_US
dc.rights İTÜ tezleri telif hakkı ile korunmaktadır. Bunlar, bu kaynak üzerinden herhangi bir amaçla görüntülenebilir, ancak yazılı izin alınmadan herhangi bir biçimde yeniden oluşturulması veya dağıtılması yasaklanmıştır. tr_TR
dc.rights İTÜ theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. en_US
dc.subject Trona tr_TR
dc.subject Sodyum Seskikarbonat tr_TR
dc.subject Sodyum Karbonat tr_TR
dc.subject Sodyum Bikarbonat tr_TR
dc.subject Flotasyon tr_TR
dc.subject Manyetik Ayırma tr_TR
dc.subject Trona en_US
dc.subject Sodium Sesquicarbonate en_US
dc.subject Sodium Carbonate en_US
dc.subject Sodium Bicarbonate en_US
dc.subject Magnetic Seperation en_US
dc.title Beypazarı Ve Kazan Trona Cevherlerinin Flotasyon Ve Manyetik Ayırma Yöntemleriyle Zenginleştirilmesi tr_TR
dc.title.alternative Processing Of Beypazari And Kazan Trona By Flotation And Magnetic Separation Methods en_US
dc.type Master Thesis en_US
Dosyalar
Orijinal seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.alt
Ad:
8162.pdf
Boyut:
7.85 MB
Format:
Adobe Portable Document Format
Açıklama
Lisanslı seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.placeholder
Ad:
license.txt
Boyut:
3.16 KB
Format:
Plain Text
Açıklama