Yayın: Scheelite flotation: a new scheme using oleoyl sarcosine as collector and alkyl oxine as modifier
| dc.contributor.author | Ozcan, O. | |
| dc.contributor.author | Bulutcu, A.N. | |
| dc.contributor.author | Sayan, P. | |
| dc.contributor.author | Recepoglu, O. | |
| dc.date.accessioned | 2026-01-25T02:05:32Z | |
| dc.date.issued | 1994-10-01 | |
| dc.description.abstract | Abstract Scheelite was selectively floated from a low-grade calcitic run-of-mine ore (containing 0.28% WO 3 , 96.3% CaCO 3 and 2.24% SiO 2 ) with a 70.6% WO 3 grade and a 70% recovery, using oleoyl sarcosine as collector, quebracho as depressant and alkyl oxine as modifier. A new scheme was developed in laboratory scale experiments to reach this grade and recovery. The scheme consisted of a slime floating stage by only frother addition upon conditioning the pulp with alkyl oxine, a regular flotation stage of scheelite by sarcosine addition and a shaking table operation to the final scheelite concentrate. | |
| dc.description.uri | https://doi.org/10.1016/0301-7516(94)90023-x | |
| dc.description.uri | https://dx.doi.org/10.1016/0301-7516(94)90023-x | |
| dc.identifier.doi | 10.1016/0301-7516(94)90023-x | |
| dc.identifier.endpage | 120 | |
| dc.identifier.issn | 0301-7516 | |
| dc.identifier.openaire | doi_dedup___::4a77bcdc4fe47361eaa9aaceedcaed34 | |
| dc.identifier.orcid | 0000-0003-4407-6464 | |
| dc.identifier.startpage | 111 | |
| dc.identifier.uri | https://hdl.handle.net/11527/42344 | |
| dc.identifier.volume | 42 | |
| dc.language.iso | eng | |
| dc.publisher | Elsevier BV | |
| dc.relation.ispartof | International Journal of Mineral Processing | |
| dc.rights | CLOSED | |
| dc.title | Scheelite flotation: a new scheme using oleoyl sarcosine as collector and alkyl oxine as modifier | |
| dc.type | Article | |