Yayın: The effect of surface treatments on the interlaminar shear failure of GLARE laminate included AA6061-T6 layers by comparing failure characteristics
| dc.contributor.author | Ucan, Cem | |
| dc.contributor.author | Süsler, Sedat | |
| dc.contributor.author | Türkmen, Halit Süleyman | |
| dc.contributor.author | Bora, Mustafa Özgür | |
| dc.date.accessioned | 2026-01-26T01:05:46Z | |
| dc.date.issued | 2022-09-07 | |
| dc.description.abstract | The effect of surface treatments on hot-pressed GLARE 3/2 laminates included AA6061-T6 is evaluated in this paper. Sandpapering, degreasing and both degreasing and sandpapering are applied on AA6061-T6 sheets in order to contribute the improvement of the interlaminar shear strength (ILSS). The three-point bending tests are carried out by using two different span length-to-specimen thickness ratios (S/h) to examine also the effect of shear and bending on deformation and failure characteristics. Strength values and failure modes are obtained for both S/h ratios and all surface treatment types. Load-displacement and stress-displacement curves are evaluated. The results show that the maximum shear strength values for surface-treated laminates are increased by between 29% and 37% against untreated one. It is observed that the strength values and failure modes of all surface-treated GLARE laminates are influenced by an increase in the S/h ratio from 4.0 to 10.0 because of the increase in bending effect against shear. | |
| dc.description.uri | https://doi.org/10.1080/09276440.2022.2120739 | |
| dc.description.uri | https://avesis.kocaeli.edu.tr/publication/details/f5c2a9b0-a8f4-4b62-b69a-d8400bd36049/oai | |
| dc.identifier.doi | 10.1080/09276440.2022.2120739 | |
| dc.identifier.eissn | 1568-5543 | |
| dc.identifier.endpage | 643 | |
| dc.identifier.issn | 0927-6440 | |
| dc.identifier.openaire | doi_dedup___::b670e984d043baa1026dc96a30c3401f | |
| dc.identifier.orcid | 0000-0002-8884-6531 | |
| dc.identifier.orcid | 0000-0002-5947-8231 | |
| dc.identifier.startpage | 627 | |
| dc.identifier.uri | https://hdl.handle.net/11527/55416 | |
| dc.identifier.volume | 30 | |
| dc.language.iso | eng | |
| dc.publisher | Informa UK Limited | |
| dc.relation.ispartof | Composite Interfaces | |
| dc.rights | CLOSED | |
| dc.title | The effect of surface treatments on the interlaminar shear failure of GLARE laminate included AA6061-T6 layers by comparing failure characteristics | |
| dc.type | Article | |
| dspace.entity.type | Publication |