Demir-çelik Tesislerinden Elde Edilen Tufalden Metalik Demirin Geri Kazanımı

dc.contributor.advisor Arısoy, Cevat Fahir tr_TR
dc.contributor.author Gündoğdu, Neşe tr_TR
dc.contributor.authorID 10000938 tr_TR
dc.contributor.department Üretim Metalurjisi tr_TR
dc.contributor.department Manufacturing en_US
dc.date 2013 tr_TR
dc.date.accessioned 2013-05-21 tr_TR
dc.date.accessioned 2015-09-07T07:57:09Z
dc.date.available 2015-09-07T07:57:09Z
dc.date.issued 2013-05-21 tr_TR
dc.description Tez (Yüksek Lisans) -- İstanbul Teknik Üniversitesi, Fen Bilimleri Enstitüsü, 2013 tr_TR
dc.description Thesis (M.Sc.) -- İstanbul Technical University, Institute of Science and Technology, 2013 en_US
dc.description.abstract Kroman çelik firmasından temin edilen tufal yığını bileşim analizinden sonra kısa süreli olarak çubuklu değirmende öğütülmüş, Divriği Ermaden’den getirilen konsantre belirli oranlarda karıştırılarak 4 farklı harman haline getirilmiştir. Bu harmanlar sırası ile peletleme cihazına alınarak üzerine melasın %12’lik sulu çözeltisi-şurup püskürtülmüş, diskin hareketi ile harmanda peletler oluşmuş ardından elde edilen bu aglomerelerin mukavemetleri ölçülmüştür. Daha sonra linyit ilavesiyle, kompozit peletle aynı özelliklere sahip tabletler üretilmiş 11000C’lik sıcak fırında belli sürelerde indirgenmiştir. İndirgeme reaksiyonuna uğramış tabletlerin faz analizleri sonrasında karışımların indirgenme davranışları irdelenmiştir. Yapılan çalışmada ince öğütmeye gerek olmadan tufaller 1mm altında olacak şekilde öğütülmüş, içinde %30, %40,%50 ve %60 Konsantre cevher olan dört farklı oranda tufal ve konsantre karışımından konsantre demir cevheri oranına bağlı olarak 5-20 mm arasında peletler üretilmiştir. Boyut büyüme en çok %60 konsantre demir cevheri ve %40 tufal karışımında 20 mm olarak bulunmuştur. Yaş ve kuru basma dayanımı da 1300 gr ve 2100 gr olarak en yüksek bu karışımdan elde edilen peletlerde görülmüştür. Dört farklı karışımdan alınan hammaddeden elde edilen tabletlerde en yüksek indirgeme süresi ve oranı olarak %30 Konsantre cevher ve %70 Tufal bileşimine sahip karışımda görülmüş, tufal miktarı arttıkça redüksiyon oranında artış olmuştur. Karışımın 20. dakika sonunda %92,83 metalizasyon derecesine ulaştığı tespit edilmiştir. %60 Konsantre cevher ile %40 Tufal karışımında 60 dakika sonunda metalizasyon oranı %88’de kalmıştır. tr_TR
dc.description.abstract Scale mass ordered from Kroman Steel has been ground in rod mills in a short time, mixed with fine ores supplied from Divriği Ermaden by several ratios and brought back 4 different mixtures. The molasses solution had been sprayed on mixture which were put on pellet disks in an order. As soon as volution of disk agglomerates were occured after that the wet and dry strengths were measured. After concluding pelletising mechanism, the composite tablets, which have same qualifications with composite pellets, had been produced by adding lignite coal and provided to reduce in furnace within 1100 degree Celcius at definite times. After taking results of reduction and phase analysis, the reduction were argued and made conclusions. The mill scales were ground undersized 1 mm, mixed within four different ratios 30%, 40%, 50% and 60% fine ore concentrates, produced pellets between 5 and 20 mm in size depending fine ore concentrate ratio. The size growth had been measured the biggest in the mixture of 60% fine ore and 40 also % mill scales as 20 mm. Also the highest wet and dry strength values were found by 1300 gr and 2100 gr. The highest iron metallisation rate had been noticed in the mixture of %30 fine ore concentrate and 70 % mill scales from composite tablets. The metallisation rate had reached 92,83 % at the end of 20 minutes in that composition, but reduction rate stayed 88% by the end of 60 minutes of 60% fine ore and 40% mill scale composition briquettes. It is observed from reduction experiment that higher present mill scales in mixtures having higher metallisation ratio. This may be because of crystalline structure of iron oxides in mill scales reducing metallic iron faster than ore concentrates. en_US
dc.description.degree Yüksek Lisans tr_TR
dc.description.degree M.Sc. en_US
dc.identifier.uri http://hdl.handle.net/11527/9184
dc.publisher Fen Bilimleri Enstitüsü tr_TR
dc.publisher Institute of Science and Technology en_US
dc.rights İTÜ tezleri telif hakkı ile korunmaktadır. Bunlar, bu kaynak üzerinden herhangi bir amaçla görüntülenebilir, ancak yazılı izin alınmadan herhangi bir biçimde yeniden oluşturulması veya dağıtılması yasaklanmıştır. tr_TR
dc.rights İTÜ theses are protected by copyright. They may be viewed from this source for any purpose, but reproduction or distribution in any format is prohibited without written permission. en_US
dc.subject Tufal tr_TR
dc.subject Konsantre cevher tr_TR
dc.subject Redüksiyon tr_TR
dc.subject Kompozit pelet tr_TR
dc.subject Yaş ve kuru basma dayanımı tr_TR
dc.subject Mill scale en_US
dc.subject Fine ore en_US
dc.subject Reduction en_US
dc.subject Composite tablet en_US
dc.subject Wet and dry tensile strength en_US
dc.title Demir-çelik Tesislerinden Elde Edilen Tufalden Metalik Demirin Geri Kazanımı tr_TR
dc.title.alternative Recycling Of Iron By Steel Mill Scales Obtained From Iron-steel Plants en_US
dc.type Thesis en_US
dc.type Tez tr_TR
Dosyalar
Orijinal seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.alt
Ad:
13500.pdf
Boyut:
4.03 MB
Format:
Adobe Portable Document Format
Açıklama
Lisanslı seri
Şimdi gösteriliyor 1 - 1 / 1
thumbnail.default.placeholder
Ad:
license.txt
Boyut:
3.14 KB
Format:
Plain Text
Açıklama