Publication: The effect of titanium on the abrasion resistance of 15Cr–3Mo white cast iron
| dc.contributor.author | Arikan, M.M | |
| dc.contributor.author | Çimenoğlu, H. | |
| dc.contributor.author | Kayali, E.S | |
| dc.date.accessioned | 2026-01-24T23:46:28Z | |
| dc.date.issued | 2001-02-01 | |
| dc.description.abstract | Abstract The influence of titanium additions up to 0.38% and heat treatment on the abrasion resistance of a commercial 15% Cr–3% Mo white cast iron were examined. The wear resistance of as-cast commercial alloy was improved about 30% by addition of 0.38% titanium after austenising at 1050°C for 6 h and quenching in air. Tempering of quenched alloys at 250°C for 6 h yielded a decrease in hardness and abrasion resistance relative to the as-quenched condition. | |
| dc.description.uri | https://doi.org/10.1016/s0043-1648(00)00523-8 | |
| dc.description.uri | https://dx.doi.org/10.1016/s0043-1648(00)00523-8 | |
| dc.identifier.doi | 10.1016/s0043-1648(00)00523-8 | |
| dc.identifier.endpage | 235 | |
| dc.identifier.issn | 0043-1648 | |
| dc.identifier.openaire | doi_dedup___::3777fe2150aee76e7f45e3f94305c97b | |
| dc.identifier.orcid | 0000-0002-9921-7108 | |
| dc.identifier.startpage | 231 | |
| dc.identifier.uri | https://hdl.handle.net/11527/39834 | |
| dc.identifier.volume | 247 | |
| dc.language.iso | eng | |
| dc.publisher | Elsevier BV | |
| dc.relation.ispartof | Wear | |
| dc.rights | CLOSED | |
| dc.title | The effect of titanium on the abrasion resistance of 15Cr–3Mo white cast iron | |
| dc.type | Article | |
| dspace.entity.type | Publication |