Publication: Enrichment of W2B5 from WO3 and B2O3 by Double SHS Method
Loading...
Date
Authors
Advisor
Department
Journal Title
Journal ISSN
Volume Title
Publisher
Kaunas University of Technology (KTU)
Type
Abstract
A second self-propagating high-temperature synthesis (SHS) was carried out to enrich the W2B5 content in the SHS product containing a mixture of various tungsten boride compounds. In the experiment, the process called Double-SHS (D-SHS) was conducted in two steps. In the first SHS reaction, an initial molar composition ratio of WO3:B2O3:Mg mixture was selected as 1:3:8. The product was then hot-leached with hydrochloric acid to eliminate MgO and Mg3B2O6 phases. The leached product, consisting of 72.6 wt.% W2B5, 16.1 wt.% WB, 8.4 wt.% W2B, and 2.9 wt.% W, was again reacted with the Mg and B2O3 mixture by second SHS. After another acid leaching step, W2B5 content in the D-SHS product was found to be 98.2 wt.%. The study showed that D-SHS is an effective method for boron enrichment in the tungsten compounds.DOI: http://dx.doi.org/10.5755/j01.ms.24.1.17834
Description
Journal or Series
Materials Science
ISSN
1392-1320
ISBN
Rights
OPEN
Keywords
leaching, Mining engineering. Metallurgy, XRD, WO3, double SHS, TN1-997, W2B5