<link rel="stylesheet" href="styles.cf390c6bfbe7555f.css">

Publication:
The effect of sulphur on tungsten recovery from scheelite concentrates by alkali fusion

Loading...
Thumbnail Image

Date

Institution Authors

Advisor

Department

Journal Title

Journal ISSN

Volume Title

Publisher

Type

Research Projects

Organizational Units

Journal Issue

Abstract

A low-grade scheelite concentrate, obtained from Uludag Tungsten Plant (Bursa, Turkey), was used in this study. It contained approximately 35% WO3, 5.2% Sand 27% Fe. The optimum conditions of alkali fusion were: a temperature of 900°C, twice the stoichiometrically required Na2CO3, and 1 h treatment time. Tungsten was dissolved with a maximum efficiency at the end of 1 h of leaching with water at a solid/liquid weight ratio of 1/5 at 80°C under continuous stirring. A dissolution efficiency of 97% was obtained when the sulphur content of scheelite concentrate was decreased to 0.7% by roasting in a rotary furnace operating at 750°C and with 100% excess amount of air, while only 78% of tungsten dissolution efficiency could be reached when the original scheelite concentrate was not roasted prior to the alkali fusion. Phase analyses showed that the sulphur in concentrate has formed a matte phase as Na3FeS3 and confined some part of the tungsten as CaWO4, during the alkali fusion, and decreased its dissolution efficiency.

Description

Journal or Series

ISSN

ISBN

Rights

closedAccess

Keywords

Citation

Collections

Endorsement

Review

Supplemented By

Referenced By

Related Patent

Related Goal

Google Scholar
Scholar'da Ara ↗
Altmetric
Dimensions
PlumX Metrikleri
BIP! Indicators