Abstract

The purpose of this study was to investigate the effects of Nd:YAG laser, air abrasion and acid-etching on the porcelain surface and repairment. Ten standard cylindrical specimens were made for each preparation (Finesse Dentsply). The specimens were lased for five seconds at a fluence of 80 mJ and a frequency of 20 Hz; air abraded for five seconds with 50 micron Al-oxide (at 60 psi); and acid etched with % 9,6 hydrofluoric acid for 120 seconds. The specimens were examined in the scanning electron microscopy (SEM) before and after the Nd:YAG laser, air abrasive and acid-etching. After silane coupling agent was applicated, two flowable restorative materials (Admira Flow, Voco; Tetric Flow, Vivadent) were bonded to the porcelain surfaces. Each group was stored in distilled water at 37oC for one day before the determination of shear bond strengths. A shear bond strength machine with 50 kg load cell and a 0.5 mm/min crosshead speed was used. The results were analyzed statistically. There was a significance between the shear bond strenth values of Admira Flow and Tetric Flow in the lased group (p<0.05). Introduction Metal-ceramic crowns combine the beauty of porcelain and the strength of metal alloys in a single restoration. Although the strength of porcelain and the bond strength of the metal substrate have improved greatly, some failures still occur under clinical conditions. The main reason for porcelain fracture is inadequate tooth preparation which results in very small interocclusal space for the metal substructure and porcelain [1]. Remaking of the crown or fixed partial denture is often inadvisable, and intraoral repair with a composite resin may be indicated [2-4]. Several intraoral porcelain repair systems are available but most of them have been only moderately succesful. Clinical procedures for nearly all systems have been complex and time consuming. Succesful repair has been an even greater problem with the metal substructure has been exposed. In this study, in vitro repair system has been evaluated. The porcelain repair systems consist of flowable composite resins (Admira Flow, Voco; and Tetric Flow, Vivadent) were used as repair materials. Materials and Methods The materials used in this study are shown in the Table 1. Porcelain discs (10 mm diameter x 3 mm) were fabricated on base metal cylinders in a porcelain furnace. The porcelain discs were then embedded in chemical-cured acrylic resin cylinders (Meliodent, Bayer) with the dimensions of 35 mm in diameter x 23 mm in height. The porcelain surfaces were polished with #600 silicon carbide papers. The porcelain specimens were divided into three groups and each group was subjected to one of the following procedures: 1) lased for five seconds at a fluence of 80 mJ and a frequency of 20 Hz; 2) air abraded for five seconds with 50 micron Al-oxide (at 60 psi); and 3) acid etched with %9,6 hydrofluoric acid for 120 seconds (Finesse All-ceramic; Dentsply, USA). Key Engineering Materials Vols. 264-268 (2004) pp. 2039-2042 online at http://www.scientific.net © (2004) Trans Tech Publications, Switzerland All rights reserved. No part of contents of this paper may be reproduced or transmitted in any form or by any means without the written permission of the publisher: Trans Tech Publications Ltd, Switzerland, www.ttp.net. (ID: 160.75.44.253-19/09/06,09:55:54) Table 1. Materials used in this study. Material Name Material Type Manufacturer Admira Flow Ormocer based flowable resin Voco, Germany Composite Tetric Flow Flowable hybrid composite Ivoclar Vivadent, Liechtenstein Admira Bond Ormocer based bonding agent Voco, Germany Bonding agent Excite Light-curing bonding agent Ivoclar Vivadent, Liechtenstein Acid Finesse All-ceramic Ceramic etchant Dentsply, USA Silane agent Silane Silane coupling agent Pulpdent Corp., USA Ceramic Finesse Low-fusing fine grain porcelain Dentsply, USA Air abrasive K.C.P. Air abrasive American Dental Tech., USA Laser Nd:YAG Laser Dental laser American Dental Tech., USA The surfaces of the specimens of each group were observed using a scanning electron microscope (SEM) before and after the Nd:YAG laser, air abrasive and acid-etching. The specimens were carbon coated under vacuum. SEM investigations were carried using a JEOL JSM-T330 scanning electron microscope operated at 15 kV. Then silane agent was applied on the porcelain surface for 30 s, which was dried with compressed air for 15 s. The three major gropus of the specimens were divided into two subgroups, and two different bonding agents (Admira Bond, Voco, Germany; Excite, Ivoclar Vivadent, Liechtenstein) were applied on the porcelain surfaces according to restorative resin to be applied. The bonding agents were polymerized for 20 seconds by using a light-curing unit (Hilux) with a light intensity of 600 mW/cm. A transparent plastic ring (3 mm diameter x 2 mm height) was placed on the specimens surface. The ring was filled with flowable composite resin and polymerized for 40 seconds by using the light-curing unit. Two different flowable composite resins were used for each major groups: Admira Flow for one subgroup, and Tetric Flow for the other subgroup. After curing the resin, the plastic ring was removed. The specimens were stored in distilled water for one day at 37 °C. Following the storage period, the shear bond strength of the bonded composite resins was determined. A shear bond strength machine (AMSLER 2 KN Tensometer, Alfred J. Amsler & Co. Switzerland) with a 50 kg load cell and a 0.5 mm/min crosshead speed was used as seen in Fig. 1.

Description

Journal or Series

Key Engineering Materials

ISSN

ISBN

Rights

CLOSED

Keywords

Citation

Collections

Endorsement

Review

Supplemented By

Referenced By

Related Patent

Related Goal

Google Scholar
Scholar'da Ara ↗
Altmetric
Dimensions
PlumX Metrikleri
BIP! Indicators