Publication: Comparative analysis of bismaleimide matrix composites reinforced with carbon fibre and quartz fibre: Mechanical properties, anisotropy, and damage mechanisms
Loading...
Date
Authors
Advisor
Department
Journal Title
Journal ISSN
Volume Title
Publisher
Iop publishing
Type
Abstract
Abstract Two bismaleimide (BMI) matrix composite systems, unidirectional carbon-fibre/BMI (CF/BMI) and woven quartz-fibre/BMI (QF/BMI), were fabricated via vacuum-assisted resin transfer moulding and evaluated under tensile (ASTM D3039), three-point flexural (ASTM D7264), Charpy impact (ASTM D6110) and short beam shear (ASTM D2344) testing in the 0° and 90° ply orientations. The CF/BMI system exhibited pronounced mechanical anisotropy across all loading modes: tensile strengths of 876 ± 36 MPa (0°) versus 17.9 ± 3.3 MPa (90°), flexural strengths of approximately 955 MPa (0°) versus 34 MPa (90°), and Charpy impact energies of 10.0 ± 0.8 J (0°) versus 1.8 ± 0.2 J (90°). The QF/BMI system displayed a near-isotropic in-plane response under quasi-static loading, with anisotropy ratios not exceeding 1.4:1 in both tensile and flexural testing; however, the Charpy impact anisotropy ratio (∼2.1:1; 3.8 ± 0.3 J versus 1.8 ± 0.3 J) was markedly higher, a trend whose underlying mechanism could not be determined from the present data set and which requires dedicated rate-sensitivity investigations. Under transverse (90°) loading, both systems converged to comparable impact energies (∼1.8 J), indicating that 90° dynamic resistance is governed predominantly by the BMI matrix rather than fibre type. Short beam shear testing yielded interlaminar shear strength values of 60.1 ± 0.3 MPa and 4.64 ± 0.07 MPa for the CF/BMI system in the 0° and 90° orientations, respectively, reflecting a strongly orientation-dependent response, whereas the QF/BMI system displayed a near-isotropic interlaminar response of 19.4 ± 0.5 MPa (0°) and 16.1 ± 0.6 MPa (90°), consistent with the balanced plain-weave architecture. Fractographic analysis identified fibre pull-out and interlaminar delamination as the dominant damage mechanisms in CF/BMI composites, whereas QF/BMI specimens exhibited matrix-dominated fracture with a preserved woven-ply architecture across all loading modes.
Description
Journal or Series
Materials research express
ISSN
ISBN
Rights
openAccess